White High Strength Net

YarnMesh DiameterWeightShadePorosityBurst Strength
Polyester1/8"8.5 oz/sq.yd.30%50%390 psi
ModelColorsDimensions (imperial)Dimensions (metric)lb/roll
SCAF4M50-WWhite12’ x 165’ = 2000 ft23.7 m x 50 m = 185 m2130 lb
  • Super strong – our toughest net for containing heavier falling debris ✓
  • Provides excellent debris & dust control as well as shade ✓
  • Diamond pattern mesh improves wind flow ✓
  • Catch light debris falling from scaffolds, bridges & buildings under construction ✓
  • Hundreds of rolls in stock at all times available for immediate shipment ✓
  • Many sizes available ✓
  • Each roll is individually bagged ✓
  • Passes NFPA 701-2004 Test Method 2 – Flame Propagation
  • Reinforced yellow buttonhole borders
  • All Scafnet® models can be quickly cut to size without fraying
  • Disposable nylon quick-ties allow for rapid Scafnet installation
  • Install bands of Scafnet® from top-to-bottom or left-to right
TestTest TypeWhite Net
1Mesh Breaking Strength (length)255 lb.
Mesh Breaking Strength (width)173 lb.
Elongation at break (length)51%
Elongation at break (width)141%
2Yarn Breaking Strength16 lb.
3Burst Strength390 psi
4Wounded Burst Strength91 psi

Description of Tests

  1. Breaking Strength of Fabrics (Grab Method: CAN/GSB-4.2 Method 9.2-M90). A 4″ wide x 6″ tall specimen of fabric is held between 2 vertical clamps. Tension is applied so that rupture of the specimen occurs within 20 seconds. This test is similar to ISO 5082:1982.
  2. Breaking Strength of Yarns (Single Strand Method: CAN/GSB-4.2 Method 9.4-M91). A single strand of yarn is held between 2 clamps. Tension is applied so that rupture of the specimen occurs within a specified interval of time.
  3. Burst Strength (Diaphragm Pressure Test: CAN/GSB-4.2 Method 11.1-94). A fixed area of fabric is subjected to pressure on one side through a diaphragm, and the pressure is gradually increased until the fabric is ruptured. This test is technically equivalent to ASTM D 3786-87.
  4. Wounded Burst Strength (Diaphragm Pressure Test: CAN/GSB-4.2 Method 11.1-94). Same as previous except a 12.5 mm cut is made to the test area.


Detailed test reports are available for all nets.